一、性能介绍Features

    具有硬化后Tg值高,CTE值低,易磨板且磨板后凹陷小等特性,适用于MLB/POFV(VOP)等电路板

    With high Tg values after curing, low CTE values, easy scrubbing and sag of small features after scrubbing, suitable for MLB/POFV (VOP) of PCB.

技术资讯Specification:

产品名称 

Product name               

项目Items

HT-50 SK-2800 G9A11

颜色
 Color

乳白色

Milky white

粘度(主剂)
 Viscosity(main agent)

25℃,粘度计/Viscometer VT-06

450~750 dPa.s(20~25℃)

比重
 Specific gravity

1.5-1.8g/cm3

CTE

α

≤45ppm

β

≤140ppm

烘烤参数
 Curing condition

TH<1.0mm

150℃×60min

1.0mm≤TH<3.0mm

95℃×10min+110℃×30min+ 150℃×50min

TH≥3.0mm

90℃×30min+110℃×30min+150℃×30min

保存期限
 Shelf life

90天(0-5℃以下储藏)
 90days(storage in 0-5℃)

附着力
 Adhesion

100/100

铅笔硬度
 Hardness

6H

包装
 Potting

1kg/
 1kg/ pot

三、操作程序Process recommendations:

                  产品名称

Product  name                  项目Items

HT-50 SK-2800 G9A11

生产参数
 Production parameters

解冻

Cooling

常温条件下放置6小时

Place 6 hours at room temperature

4-6小时

4-6hours

搅拌

Mixing

不搅拌或真空搅拌

Use as it is or after vacuum stirring

30-45min.

印刷条件

Printing condition

网塞,铝片或真空机塞

Mesh plug, aluminium sheet or vacuum machine


刮刀

Squeegee

硬度 Hardness

70N

厚度 Thickness

20mm

角度 Angle

5-10

5-10degree

压力 Pressure

5-10Mpa

速度 Speed

20-100mm/s

硬化条件Curing condition

TH<1.0mm

150℃×60min


1.0mm≤TH<3.0mm

95℃×10min+110℃×30min+ 150℃×50min


TH≥3.0mm

90℃×30min+110℃×30min+150℃×30min


整平 leveling

内层,次外层板 inner layer, outer layer


打磨 Polish

1-3次   1-3times


注意事项:
 a. 建议在温度为20-25度,湿度50-60%RH的无尘环境内操作。
 b. 因每间工厂的烘干设备,生产条件和品质要求各有不同,烘干温度及时间也有所不同,请进行实验,测试后方可生产。
 c. 如果发现油墨变粘或无法搅拌时,表明油墨已经过期或因储存不当而变质,应立即进行油墨的更换。

Notes:
 A
. Recommended in the temperature of 20-25  degrees, humidity 50-60%RH clean environment operation
 B. Because each factory's drying equipment, production  conditions and quality requirements are different, drying temperature and  time are also different, please do the experiment, after the test can be  produced.

C.  if the ink becomes sticky or unable to stir, indicates that the ink has expired  or because of improper storage and deterioration, should be immediately  replaced by ink.

注明:以上为建议参数,现场使用时请根据自身工艺设备的实际情况进行调整。

Note: the above is the recommended parameters, on-site use, according to the actual situation of their own equipment to adjust.